DENTSPLY Megalloy EZ Instrucciones De Uso página 2

Cápsula de autoactivación de aleación esférica
Ocultar thumbs Ver también para Megalloy EZ:
Tabla de contenido
Idiomas disponibles
  • ES

Idiomas disponibles

8. STEP-BY-STEP INSTRUCTIONS
1. Treatment of the preparation: Clean freshly instrumented enamel and dentin with water
spray and then air dry. The use of pulpal protection, bases and/or cavity liners is at the
discretion of the operator, as dictated by the clinical presentation. If desired, Megalloy
Amalgam may be placed over an adhesive liner or adhesively bonded by following the
manufacturer's instructions for compatible adhesive systems (available separately).
2. Trituration: Simply place Megalloy
®
amalgamator. These capsules are activated by the amalgamator – they do not require manual
activation. Trituration speed and time is an important factor in preparing the amalgam, in
order to achieve proper amalgam mix consistency. The chart that follows provides guidelines
in determining amalgamator trituration time and speed setting for Megalloy
Self-Activating Capsules:
Approximate Trituration Time Range (in seconds)
Amalgamator
Caulk ProMix
®
Caulk Vari-Mix
®
II M
Caulk Vari-Mix
®
III
Wig-L-Bug MSD
Wig-L-Bug LPD
*Kerr AutoMix
*ADEC Model 6440
*Pelton & Crane Spirit Model SM
*Zenith Stirspeed Model TP-103
*Zenith Stirspeed Model Z-1A
*Vivadent Silamat Plus
*Vivadent Silamat Plus 220V
*SDI Ultramat 2
*ESPE CapMix
*Torit Capmaster
The following amalgamators are not recommended for use with Megalloy
Activating Capsules: *ESPE Rotamix and *Torit Single Speed Amalgamator Model TRA-18-1
*Not products of DENTSPLY International.
Suggestions for obtaining optimum mix
2.1 The triturated amalgam should be bright and have a plastic consistency. If the amalgam
is excessively splashy and wet looking, INCREASE trituration time or amalgamator
speed. Amalgam that appears excessively dry indicates trituration time or amalgamator
speed should be DECREASED. Slow speed amalgamators are not recommended.
2.2 When performing adjustments, it is recommended to adjust trituration time in 2 second
increments, until optimum mix is obtained. Greater adjustments may indicate
amalgamator incompatibility or compromised functionality.
Decrease trituration time:
- To lengthen working time
- If mix is too hot
- If mix is too dry
2.3 Properly triturated Megalloy
®
EZ Amalgam does not require mulling to produce a smooth
plasticity; however you may mull for 1-2 seconds after removing pestle to collect
amalgam into a single mass.
EZ Amalgam Self-Activating Capsules in the
Speed
1 Spill
2 Spill
Rabbit (4200 cpm)
7-9
M2 (3900 cpm)
7-9
M (3900 cpm)
7-10
7-10
3800 cpm
8-11
8-11
3800 cpm
9-11
9-11
4000 cpm
10-13
10-13
#7 (4200 cpm)
9-13
10-15
4000 cpm
12-15
12-15
Fixed 3950 cpm
8-11
10-12
H 4100 cpm
7-11
7-12
Fast 4700 cpm
6-8
Fast 4700 cpm
7-9
7-10
4400 cpm
8-12
8-12
Fixed 4400 cpm
8-10
8-10
4200 cpm
10-14
10-14
®
EZ Amalgam in Self-
Increase trituration time:
- To shorten working time
- If mix is too wet
3. Condensation
3.1 No tool is needed to open the Self-Activating capsule. Just grasp both ends of the
capsule, twist, and pull apart. Turn the opened capsule upside down to drop the
amalgam mass into the work area. Megalloy
®
EZ
placement and condensation. A gentle tap may be required to free amalgam from the
capsule. Do not attempt to manually express mercury from the triturated mass prior to
placement.
3.2 A plastic wafer and/or plastic mixing pestle may be seen. These have no further function
and should be properly recycled.
3.3 Condense immediately after mix is completed. Use a clean amalgam carrier to transfer
increments to the cavity. Pack each increment into angles and undercuts with small-
®
EZ Amalgam
faced plugger and sufficient pressure to insure good adaptation. Build the restoration
with additional portions, until the cavity is slightly overfilled. Remove any mercury-rich
amalgam from the surface that may develop during condensation.
4. Carving/Burnishing: Carving can begin immediately after condensation. A sharp carver will
3 Spill
give best results. The anatomy should be carved proceeding from the proximal margins
7-9
8-10
towards the center of the restoration. Before the matrix band is removed, the marginal ridge
should be supported by a condenser. After removal of the matrix band, gingival margins may
7-9
8-10
be smoothed with a curved explorer. Burnishing setting amalgam is recommended to improve
9-12
surface smoothness.
10-12
5. Polishing: The quality of the Megalloy
9-11
polishing. The amalgam should be allowed to set 24 to 48 hours before polishing. See
selected polishing instrument manufacturer's directions for use.
9-12
10-15
Hygiene
13-16
• Cross-contamination
• Do not reuse single use products. Dispose in accordance with local regulations.
10-12
10-13
6-9
7-9
9. LOT NUMBER AND EXPIRATION DATE
1. Do not use after expiration date. ISO standard is used: "YYYY/MM"
7-10
2. The following numbers should be quoted in all correspondence.
7-10
• Reorder number
9-12
• Lot number on package
10-14
• Expiration date on package
®
EZ amalgam is now ready for immediate
®
EZ Amalgam restoration will be enhanced by
Manufactured by:
Distributed by:
DENTSPLY Caulk
DENTSPLY Canada
38 West Clarke Avenue
161 Vinyl Court
Milford, DE 19963 USA
Woodbridge, Ontario
Tel.: 1-302-422-4511
L4L 4A3 Canada
www.dentsply.com
©2010 DENTSPLY International. All rights reserved.
DENTSPLY D
T
GmbH
E
REY
De-Trey-Str. 1
78467 Konstanz, Germany
Tel.: 49-7531-583-0
www.dentsply.de
Form #503051 (R 4/16/10)
Tabla de contenido
loading

Tabla de contenido