Preparation Of The Coating Material; Start-Up - WAGNER W 600 Manual De Uso

Tabla de contenido
Idiomas disponibles

Idiomas disponibles

W 600

Preparation of the Coating Material

The W 600 can be used to spray paints, varnishes and glazes that are undiluted or slightly
diluted . Detailed information is available in the technical data sheet of the manufacturer
( Internet Download) .
1. Stir the material up and put the required amount into the paint container .
Sprayed material
Glazes
Wood preservatives, mordants, oils, disinfection agents,
plant protective agents
Paints containing solvents and water-soluble paints,
primers, thick-film glazes
2. If the convey capacity is too low, add 5 - 10 % dilution step-by-step until the convey
capacity fulfils your requirements .

Start-up

Before connecting to the mains supply, be sure that the supply voltage is identical with
the value given on the rating plate .
A ttach the carrying strap to the unit . (Fig. 2)
U nscrew the container from the spray gun .
A ligning suction tube . (Fig. 3)
If the suction tube is positioned correctly, the container contents can be sprayed
without almost any residue .
When spraying horizontal surfaces, turn suction tube forward . (Fig . 3 A)
When spraying objects overhead, turn suction tube back . (Fig . 3 B)
S et the container on a sheet of paper, pour in the prepared coating material and
screw the container tightly onto the spray gun .
M ount the air hose (Fig . 4, a + b) . Insert the air hose firmly into the connection of the
unit and the gun handle . The position of the hose is not relevant .
I nsert the spray gun into the gun holder on the unit .
P ut the machine down only on a level, clean surface . Otherwise, the gun may suck in
dust, etc .
S ling on the carrying strap with the unit .
R emove the spray gun from the gun holder and point it at the object to be coated .
I t is advisable to test spray cardboard or a similar material in order to determine the
material quantity and the spray pattern .
P ress the ON/OFF switch at the device .
thinning recommendation
GB
undiluted
undiluted
dilute by 5 - 10 %
29