GYS NEOFEED 4W Manual Del Usuario página 47

Tabla de contenido
Idiomas disponibles

Idiomas disponibles

4-
Full traceability
- ON
Pass (ON/OFF)
Welding (ON/OFF)
Temperature (ON/OFF)
Length (ON/OFF)
5-
Project/bead display
At the top left, the project name and
bead number are displayed.
(The bead number is automatically
incremented and cannot be modified)
The «Explore» function allows you to access the list of work sessions created, sort them and also delete them.
The pictogram
shows the details of each session with the following information: sampling frequency, number of recorded beads, total
welding time, welding current supplied, configuration of each bead (process, time stamp, welding time and welding U-I).
The transfer of this information is done by exporting the data to a USB key.
The CSV data can be processed using spreadsheet software (Microsoft Excel
ENERGY MODE
This mode developed for welding with energy control framed by a DMOS allows, in addition to the energy display of the bead after welding, to set:
The thermal coefficient according to the standard used: 1 for ASME standards and 0.6 (TIG) or 0.8 (MMA/MIG-MAG) for European standards. The
displayed energy is calculated by taking this coefficient into account.
TROUBLESHOOTING, CAUSES, SOLUTIONS
SYMPTOMS
The wire feed is not constant.
The wire feed motor does not work.
NEOFEED 4W
Definition :
• A welding CORD corresponds to a welding cycle.
• The PASS corresponds to welding over the entire perimeter of the part to be welded.
• The WELD is the end junction of the two joined up plates. The weld is therefore made of
one or more passes.
• The PROJECT is made of one or more finished welds.
• Temperature
ON : Temperature of the plate to be welded at the beginning of the cord.
*
• Length* ON : Cord length
the measurement units are displayed based on the selection defined in PARAMETERS/Units.
*
6-
Identification
At each end of the cord, an identifica-
tion window is displayed: Pass number,
Weld number, Temperature of the plate
and/or length of the cord.
, Calc OpenOffice
®
POSSIBLE CAUSES
Debris are blocking the hole.
The wire is spinning on the rollers.
One of the rollers is spinning.
The torch cable is entangled.
The brake on the reel or roller is too tight.
7-
Validation
The validation can be done using the
interface or by pulling the trigger.
, etc.).
®
SOLUTIONS
Clean or replace the contact tip and apply an anti-
sticking solution.
Apply an anti-sticking solution.
Check the tightening of the roller screw.
The torch cable must be as straight as possible.
Loosen the brake and rollers
EN