► Shorten the prosthetic glove at the point with the largest dia
meter (at the height of the elbow).
► NOTICE! Do not use a hot air gun. Do not exceed the tem
perature or time.
Place the prosthetic glove into the oven (10 – 15 min / 60 °C).
Required materials:
>
640F18 Donning Spray
► Spray the donning sphere with donning spray immediately prior
to removal of the prosthetic glove from the oven.
► Remove the prosthetic glove from the oven and spray the inside
with donning spray.
► Pull the prosthetic glove on to the donning sphere.
► NOTICE! Do not exceed the maximum stretch time (20 s).
Place the prosthetic glove on to the donning sphere at the
height of the wrist (see dashed line).
Ottobock | 17