GYS NEOPULSE 220 C Manual Del Usuario página 35

Tabla de contenido
Idiomas disponibles

Idiomas disponibles

Energie
MIG-MAG WELDING
• GMAW/MIG-MAG Manual
Settings
Designation
Wire speed
Voltage
Self
Pre-gas
Post gaz
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.
• Standard MIG-MAG/GMAW (Dynamic STD)
The Standard mode allows high quality welding on most ferrous materials such as steel, stainless steel, but also copper and its alloys, titanium... The
many possibilities of current and gas management allow you to perfectly control your welding operation, from the priming to the final cooling of your
weld bead.
Settings
Designation
Thickness
Speed
Current
Arc length
Self
Pre-gas
Approach speed
Hot Start
Crater Filler
Post gaz
Access to some welding parameters depends on the selected display mode: Settings/User Level: Easy, Expert, Advanced.
NEOPULSE 220 C / 220 C XL
Hold
Thermal coeff.
Adjustable
settings
0.5 - 20m/min
Quantity of filler metal deposited and indirectly the welding intensity.
10 - Umax
Sets the welding power.
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 25 secs.
and the electrode against oxidisation when the metal is cooling down.
Adjustable
settings
The synergy allows for fully automatic settings. Adjusting the thickness
0.1 - 5.5 mm
automatically sets the right voltage and wire speed.
0.5 - 20m/min
Quantity of filler metal deposited and indirectly the welding intensity.
The welding current is adjusted according to the type of wire used and the material to
15 - Imax
be welded.
Used to adjust the distance between the end of the wire and the weld (voltage adjust-
-6 > +6
ment).
Smoothes more or less the welding current. To be adjusted according to the welding
-4 > +4
position.
0 - 25 secs.
Torch purge time and to protect the area with gas before ignition
Progressive wire speed. Before the arcing, the wire arrives slowly to create the first
50 - 200 %
contact without causing a jolt.
The Hot Start is an overcurrent during generated during the arcing phase to prevent
50 - 200 %
the wire from sticking. It is adjustable in intensity (% of welding current) and time
0 - 5 secs.
(seconds).
This current treshold when stopped is a phase after the current downslope.
50 - 100 %
It is adjustable in intensity (% of welding current) and time (seconds).
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 25 secs.
and the electrode against oxidisation when the metal is cooling down.
See chapter «ENERGY MODE» on pages
following.
Description & advice
Description & advice
EN
35
Tabla de contenido
loading

Este manual también es adecuado para:

Neopulse 220 c xl

Tabla de contenido