MUTLI SPOT (TIG DC or AC)
This is a scoring mode similar to the TIG SPOT, but with a combination of scoring and stopping time defined as long as the trigger is held in.
Settings
Designation
Pre-gas
Welding current
Spot
Post-gas
Duration between 2
points
AC wave shape
Frequency of
welding
Penetration and
cleaning (%)
TACK (TIG DC)
This mode can also pre-assemble workpieces, but in two phases : first phase is DC pulse whcih concentrates the arc for enhanced penetration, fol-
lowed by a DC standard phase which enlarges the arc and the weld pool for a good spot.
The adjustable duration of each phase enables control of the weld time for better spot welding results and an non-oxidised spot.
Settings
Designation
Pre-gas
Welding current
Pulsed duration
Frequency
of pulsation
Non-pulsed duration
Post-gas
42
TITANIUM 400 AC/DC
Adjustable
settings
0 - 60 sec.
Time to purge the torch and to protect the area with gas before ignition
3 - 400 A
Welding current.
Manual or a defined time.
, 0 - 60 sec.
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 60 sec.
and the electrode against oxidisation when the metal is cooling down.
Time between the end of a point (excluding PostGaz) and the recovery of a new point
0.1 - 20 sec.
(including PreGas).
AC waveform.
20 - 300 Hz
Frequency of polarity reversals welding - pickling
20 - 60%
Percentage of the welding period dedicated to pickling (default 30-35%)
Adjustable
settings
0 - 60 sec.
Time to purge the torch and to protect the area with gas before ignition
3 - 400 A
Welding current.
Manual pulsation phase or of a defined duration
, 0 - 60 sec.
0.1 - 2500 Hz
Pulse frequency
Smooth current phase manual or of a defined duration
, 0 - 60 sec.
Duration for which gas is released after the arc has stopped. It protects the weld pool
0 - 60 sec.
and the electrode against oxidisation when the metal is cooling down.
Description & advice
Description & advice
EN